IMPACT WEAR OF IRON RICH SUPERALLOYS.

  • University of Connecticut

Research output: Contribution to journal › Conference article › peer-review

Original languageEnglish
Pages (from-to)567-571
Number of pages5
JournalWear of Materials: International Conference on Wear of Materials
StatePublished - 1985