Pitting corrosion analysis of stainless steel by boundary element method with strain-dependent polarization curve

  • Osamu Kuwazuru
  • , Aruto Kawakami
  • , Yuma Miura
  • , Eduardo Divo
  • , Alain Kassab
  • University of Fukui
  • Embry-Riddle Aeronautical University
  • University of Central Florida

Research output: Contribution to journalArticlepeer-review

Original languageEnglish
Pages (from-to)51-62
Number of pages12
JournalInternational Journal of Computational Methods and Experimental Measurements
Volume9
Issue number1
DOIs
StatePublished - Mar 4 2020
Externally publishedYes

ASJC Scopus Subject Areas

  • Computational Mechanics
  • Modeling and Simulation
  • Computer Science Applications
  • Computational Mathematics
  • Applied Mathematics

Keywords

  • Boundary element method
  • Coupling problem
  • Electrochemistry
  • Mechanical damage
  • Oxide film
  • Polarization
  • Stress concentration
  • Stress corrosion

Cite this